Citric Acid Modification of Jute Fibre: Comparative Study of Alkali, Citric Acid and Sodium-Hypophosphite Assisted Treatments

  • Unique Paper ID: 209824
  • Volume: 13
  • Issue: 5
  • PageNo: 3563-3573
  • Abstract:
  • Natural lignocellulosic fibres possess attractive sustainability and specific mechanical characteristics but exhibit hydrophilicity and limited interfacial compatibility with polymer matrices. Chemical surface modification is therefore widely employed to alter fibre morphology and surface chemistry. The present study investigates the comparative effects of sodium hydroxide (NaOH), citric acid (CA), and sodium-hypophosphite-assisted citric acid (CA/SHP) treatments on jute fibre. Untreated jute, 5% NaOH-treated jute, 5% citric-acid-treated jute and 5% CA/SHP-treated jute were characterised using field-emission scanning electron microscopy (FESEM), energy-dispersive X-ray spectroscopy (EDS) and Fourier-transform infrared spectroscopy (FTIR). Particular emphasis was placed on EDS results expressed as both weight percentage and atomic percentage and on the resulting O/C ratios. Untreated jute exhibited 54.33 wt% C and 39.49 wt% O, whereas 5% CA treatment increased the oxygen content to 43.41 wt% and 37.02 at%. CA/SHP treatment produced the highest oxygen content, 43.83 wt% and 37.38 at%. The calculated atomic O/C ratio increased from approximately 0.547 for untreated jute to 0.594 and 0.603 for CA and CA/SHP treatments, respectively. NaOH treatment produced a smaller increase in atomic O/C but caused a substantial reduction in Si and Ca, indicating removal of surface-associated constituents. FESEM observations revealed increased fibrillation, longitudinal grooves and surface irregularities following chemical modification. FTIR analysis showed characteristic hydroxyl, C–H, carbonyl-related and C–O absorption bands. The combined EDS, FESEM and FTIR results indicate that citric acid produces significant oxygen-rich surface modification, with CA/SHP producing the strongest oxygen enrichment among the investigated conditions. The findings provide supporting evidence for citric-acid-induced chemical modification and potential improvement in fibre–matrix interaction.

Copyright & License

Copyright © 2026 Authors retain the copyright of this article. This article is an open access article distributed under the Creative Commons Attribution License which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.

BibTeX

@article{209824,
        author = {Aparna Kulkarni},
        title = {Citric Acid Modification of Jute Fibre: Comparative Study of Alkali, Citric Acid and Sodium-Hypophosphite Assisted Treatments},
        journal = {International Journal of Innovative Research in Technology},
        year = {2026},
        volume = {13},
        number = {5},
        pages = {3563-3573},
        issn = {2349-6002},
        url = {https://ijirt.org/article?manuscript=209824},
        abstract = {Natural lignocellulosic fibres possess attractive sustainability and specific mechanical characteristics but exhibit hydrophilicity and limited interfacial compatibility with polymer matrices. Chemical surface modification is therefore widely employed to alter fibre morphology and surface chemistry. The present study investigates the comparative effects of sodium hydroxide (NaOH), citric acid (CA), and sodium-hypophosphite-assisted citric acid (CA/SHP) treatments on jute fibre. Untreated jute, 5% NaOH-treated jute, 5% citric-acid-treated jute and 5% CA/SHP-treated jute were characterised using field-emission scanning electron microscopy (FESEM), energy-dispersive X-ray spectroscopy (EDS) and Fourier-transform infrared spectroscopy (FTIR). Particular emphasis was placed on EDS results expressed as both weight percentage and atomic percentage and on the resulting O/C ratios. Untreated jute exhibited 54.33 wt% C and 39.49 wt% O, whereas 5% CA treatment increased the oxygen content to 43.41 wt% and 37.02 at%. CA/SHP treatment produced the highest oxygen content, 43.83 wt% and 37.38 at%. The calculated atomic O/C ratio increased from approximately 0.547 for untreated jute to 0.594 and 0.603 for CA and CA/SHP treatments, respectively. NaOH treatment produced a smaller increase in atomic O/C but caused a substantial reduction in Si and Ca, indicating removal of surface-associated constituents. FESEM observations revealed increased fibrillation, longitudinal grooves and surface irregularities following chemical modification. FTIR analysis showed characteristic hydroxyl, C–H, carbonyl-related and C–O absorption bands. The combined EDS, FESEM and FTIR results indicate that citric acid produces significant oxygen-rich surface modification, with CA/SHP producing the strongest oxygen enrichment among the investigated conditions. The findings provide supporting evidence for citric-acid-induced chemical modification and potential improvement in fibre–matrix interaction.},
        keywords = {jute fibre; citric acid; sodium hydroxide; sodium hypophosphite; EDS; atomic percentage; esterification; FTIR; FESEM; natural fibre composite},
        month = {October},
        }

Cite This Article

Kulkarni, A. (2026). Citric Acid Modification of Jute Fibre: Comparative Study of Alkali, Citric Acid and Sodium-Hypophosphite Assisted Treatments. International Journal of Innovative Research in Technology (IJIRT), 13(5), 3563–3573.

Related Articles