@article{211121,
author = {Vijay Babu Gaur and Dr Harshvardhan Saraswat},
title = {Evaluating the Mechanical Stability of Cut-Resistant Woven Fabrics after Successive Laundering Cycles},
journal = {International Journal of Innovative Research in Technology},
year = {2026},
volume = {13},
number = {6},
pages = {3543-3552},
issn = {2349-6002},
url = {https://ijirt.org/article?manuscript=211121},
abstract = {Repeated laundering is an important durability consideration for reusable protective textiles because washing may alter yarn arrangement, fabric compactness and the mechanical response of the textile structure. This study evaluates the effect of five and ten repeated washing cycles on the tensile strength, tearing strength and cut-resistance force (N) of twelve woven cut-resistant fabric constructions. The fabric set comprised FSS-25, FSS-50, FSS-75 and FGF-50 yarn systems, each produced in plain, twill and sateen weaves. Laundering was carried out in an IFB Elite VX front-loading washing machine using the laundering procedure adopted from AATCC LP1:2021, at 30°C for 30 minutes per cycle. Five independent replicate specimens were evaluated for each fabric construction and washing condition. Tensile and tear strength were evaluated in warp and weft directions, while cut resistance was evaluated as force. The mean percentage reductions, averaged across fabric constructions and measured directions, were 1.84% and 3.62% for tensile strength, 1.34% and 2.64% for tear strength, and 0.91% and 1.51% for cut-resistance force (N) after five and ten cycles, respectively. A three-factor factorial ANOVA (fabric code × weave × washing condition), conducted separately for each direction, showed a statistically significant washing-cycle effect on tensile strength and tear strength (p < 0.001), whereas the washing-cycle effect on cut-resistance force was not significant (F (2,144) = 2.31, p = 0.103). Fabric code and weave construction were significant sources of variation for all three properties. The findings indicate that the tested fabrics retained most of their measured mechanical performance after ten cycles, although modest reductions occurred in tensile and tear strength. Cut-resistance force is reported in newtons (N), and the same test methods were used before and after laundering.},
keywords = {Cut-Resistant Fabrics, Factorial ANOVA, Laundering, Mechanical Properties, Tear Strength, Tensile Strength, Woven Fabrics.},
month = {November},
}